In this study, Janka-Hardness of fast grown Douglas-fir Pseudotsuga menziesii (Mirb.) Franco] were investigated. All trees used for experiments were obtained from Ayancık and samples were then prepared in accordance with the related standards. Consequently, the average janka hardness was found as 280.983 kg/cm2  An increasing relationship between specific gravity and janka hardness values was determined.

References

  • Ay, N., Duglas (Pseudotsuga menziesii (Mirb.) Franco) Odununun Anatomik, Fiziksel ve Mekanik Özellikleri, Doktora Tezi, KTÜ Orman Fakültesi, Trabzon, 1994.
  • Koltzenburg, C., Venvertung und Vervendung von Einheimischen Douglasienh Holz, Teil 2, Holzzentrall blatt, 105 (135) (1979) 2007-2009.
  • Eiselt, M.G., Nadelgehölze, Nevman Verlag, Monsehen, 1960.
  • Duglas (Pseudotsuga menziesii (Mirb.) Franco) Odununun Janka Sertlik Değeri 4. Gerstetter, L., Keller, P., Die Eignung von Geringwenigen Kiefernstammholz ausdern
  • Westdeutschen Raum für die Furnierplatten Erzeugung, Holz als Roh und Werstoff, 34 (7) (1976) 112-120.
  • Noack, O.J., Holz-eigen schaften und Verwendungs möglichkeiten Schnellwachsenden Baumarten, Der Forest und Holzwirtt, 3 (11) (1979) 112-120.
  • Milter, D.J., Permeability of Douglas Fir in Oregon, For. Prod. Journal, 12 (3) (1961) 14- 17.
  • Pechmann, C.H., Untersuchungen über die Holz Eigenschaften von Douglasien aus Einheimischen Anbaugebicten, Fortwiss- Centralbl., 89 (2) (1970) 88-122.
  • Winandy, J.E., Levan, S.L., Schaffer, E., Lee, P.W., Effect of Fire- Retardant Treatment and Redrying on The Mechanical Properties of Douglas-fir and Aspen Playwood, Research Paper-Forest Prod. Lab., USD, Forest. Service, No. FPL - RD – 485, 1988.
  • Şimşek, Y., Duglas Yetiştirme Tekniği, Ormancılık Araştırma Enstitüsü Yayınları, Muhtelif Yayınlar Serisi No:55, Ankara, 1988.
  • Bozkurt, Y., Göker,Y., Fiziksel ve Mekanik Ağaç Teknolojisi, Cilt 1, İÜ Orman Fakültesi, Yayın No: 2481/259, İstanbul, 1980.
  • Berkel, A., Ağaç Malzeme Teknolojisi, Cilt 1, İÜ Orman Fakültesi Yayın No: 1448/47, İstanbul, 1970.

DUGLAS (Pseudotsuga menziesii (Mirb.) Franco) ODUNUNUN JANKA SERTLİK DEĞERİ

Year 2005, Volume: 6 Issue: 1, 11 - 16, 20.03.2011

Abstract

Çalışmada hızlı gelişen türler içinde önemli bir yer tutan Duglas (Pseudotsuga menziesii (Mirb.) Franco) odununun janka sertlik değerinin araştırılması esas alınmıştır. Bunun için Ayancık Bölgesinden örnekler alınmış ve deneyler ilgili standartlara göre hazırlanmış örnekler üzerinde yapılmıştır. Sonuç olarak ortalama janka sertlik değeri 280.983 kg/cm2 bulunmuştur. Özgül ağırlık ile janka sertlik değeri arasında artan bir ilişki olduğu belirlenmiştir

References

  • Ay, N., Duglas (Pseudotsuga menziesii (Mirb.) Franco) Odununun Anatomik, Fiziksel ve Mekanik Özellikleri, Doktora Tezi, KTÜ Orman Fakültesi, Trabzon, 1994.
  • Koltzenburg, C., Venvertung und Vervendung von Einheimischen Douglasienh Holz, Teil 2, Holzzentrall blatt, 105 (135) (1979) 2007-2009.
  • Eiselt, M.G., Nadelgehölze, Nevman Verlag, Monsehen, 1960.
  • Duglas (Pseudotsuga menziesii (Mirb.) Franco) Odununun Janka Sertlik Değeri 4. Gerstetter, L., Keller, P., Die Eignung von Geringwenigen Kiefernstammholz ausdern
  • Westdeutschen Raum für die Furnierplatten Erzeugung, Holz als Roh und Werstoff, 34 (7) (1976) 112-120.
  • Noack, O.J., Holz-eigen schaften und Verwendungs möglichkeiten Schnellwachsenden Baumarten, Der Forest und Holzwirtt, 3 (11) (1979) 112-120.
  • Milter, D.J., Permeability of Douglas Fir in Oregon, For. Prod. Journal, 12 (3) (1961) 14- 17.
  • Pechmann, C.H., Untersuchungen über die Holz Eigenschaften von Douglasien aus Einheimischen Anbaugebicten, Fortwiss- Centralbl., 89 (2) (1970) 88-122.
  • Winandy, J.E., Levan, S.L., Schaffer, E., Lee, P.W., Effect of Fire- Retardant Treatment and Redrying on The Mechanical Properties of Douglas-fir and Aspen Playwood, Research Paper-Forest Prod. Lab., USD, Forest. Service, No. FPL - RD – 485, 1988.
  • Şimşek, Y., Duglas Yetiştirme Tekniği, Ormancılık Araştırma Enstitüsü Yayınları, Muhtelif Yayınlar Serisi No:55, Ankara, 1988.
  • Bozkurt, Y., Göker,Y., Fiziksel ve Mekanik Ağaç Teknolojisi, Cilt 1, İÜ Orman Fakültesi, Yayın No: 2481/259, İstanbul, 1980.
  • Berkel, A., Ağaç Malzeme Teknolojisi, Cilt 1, İÜ Orman Fakültesi Yayın No: 1448/47, İstanbul, 1970.
There are 12 citations in total.

Details

Primary Language English
Journal Section Eski Sayılar
Authors

Nurgül Ay

Publication Date March 20, 2011
Published in Issue Year 2005Volume: 6 Issue: 1

Cite

APA Ay, N. (2011). JANKA HARDNESS OF DOUGLAS (Pseudotsuga menziesii (Mirb.) Franco) WOOD. Artvin Çoruh Üniversitesi Orman Fakültesi Dergisi, 6(1), 11-16.
AMA Ay N. JANKA HARDNESS OF DOUGLAS (Pseudotsuga menziesii (Mirb.) Franco) WOOD. ACUJFF. March 2011;6(1):11-16.
Chicago Ay, Nurgül. “JANKA HARDNESS OF DOUGLAS (Pseudotsuga Menziesii (Mirb.) Franco) WOOD”. Artvin Çoruh Üniversitesi Orman Fakültesi Dergisi 6, no. 1 (March 2011): 11-16.
EndNote Ay N (March 1, 2011) JANKA HARDNESS OF DOUGLAS (Pseudotsuga menziesii (Mirb.) Franco) WOOD. Artvin Çoruh Üniversitesi Orman Fakültesi Dergisi 6 1 11–16.
IEEE N. Ay, “JANKA HARDNESS OF DOUGLAS (Pseudotsuga menziesii (Mirb.) Franco) WOOD”, ACUJFF, vol. 6, no. 1, pp. 11–16, 2011.
ISNAD Ay, Nurgül. “JANKA HARDNESS OF DOUGLAS (Pseudotsuga Menziesii (Mirb.) Franco) WOOD”. Artvin Çoruh Üniversitesi Orman Fakültesi Dergisi 6/1 (March 2011), 11-16.
JAMA Ay N. JANKA HARDNESS OF DOUGLAS (Pseudotsuga menziesii (Mirb.) Franco) WOOD. ACUJFF. 2011;6:11–16.
MLA Ay, Nurgül. “JANKA HARDNESS OF DOUGLAS (Pseudotsuga Menziesii (Mirb.) Franco) WOOD”. Artvin Çoruh Üniversitesi Orman Fakültesi Dergisi, vol. 6, no. 1, 2011, pp. 11-16.
Vancouver Ay N. JANKA HARDNESS OF DOUGLAS (Pseudotsuga menziesii (Mirb.) Franco) WOOD. ACUJFF. 2011;6(1):11-6.
Creative Commons License
Artvin Coruh University Journal of Forestry Faculty is licensed under a Creative Commons Attribution 4.0 International License.